Hiperco® 50 alloy heat treated between 450 and 650 °C exhibits superior mechanical properties. We report the measurements of the ac core loss at various frequencies up to 4500 Hz of the Hiperco® 50 alloy samples annealed at 450 and 650 °C. The 650 °C annealed specimens have lower ac core loss than the 450 °C annealed ones. The total core loss, consisting of contributions from hysteresis core loss and eddy-current core loss, depends on the frequency f as af+bf2. The eddy current loss of a single laminate is minor compared to the hysteresis loss.
Publisher's Statement
Copyright (2003) American Institute of Physics. This article may be downloaded for personal use only. Any other use requires prior permission of the author and the American Institute of Physics. The following article appeared in J. Appl. Phys. 93, 7121 (2003), and may be found at http://jap.aip.org/resource/1/japiau/v93/i10/p7121_s1.
Citation
X. M. Cheng et al., J. Appl. Phys. 93, 7121 (2003).
DOI
10.1063/1.1557308